Usage

 

HN- trump nickel plating feed water can take place of the softeners, assistants or feed water used in other bright nickel plating£» its brighteners are thicker with less consumption and more outstanding feeding£» when combined with the nickel plating brightener £¨such as 
HN-8, HN-6, HN-3L, HN-B, HN-BL, HN-BP, etc.£©, it can create a spotless
white and fine layer with excellent flexibility and leveling.  But it
cannot take place the softener and assistant in new working conditions.

¡¡¡¡HN- trump nickel plating feed water can decrease the layer internal stress to soften the layer. In addition, it can£º

¡ñ improve the solution dispersibility to brighten the LCD layer with a better leveling. 
¡ñ improve the tolerance against zinc, copper, iron and other impurities to extend the solution treatment cycle.  
¡ñ improve the ultra LCD coverage and deep plating to facilitate trough or deep hole plating 
¡ñ broaden the solution's working range to resist troubles. 


New area consumption: 8-10 ml/l

Conversion or Addition£º 100-150 ml/KAh