Ingredient
Hydroxide radical modified polysiloxane
Index
Appearance: |
White blue liquid |
Ionicity: |
Cation |
PH value: |
6-7 |
Stability: |
3000r/mins,30min without interlayer |
Properties and features
1, It can make the fabric soft, flexible and smooth.
2, It can make the sewing wire smooth and high abrasive resistance.
3, It reinforces the usability during the running up of sewing machine.
Application
1, It is used in the soft finishing of natural fiber, rayon , etc.
2, It can make better smoothing abrasive resistance
Using method
1,Padding:20-30g/L silicon emulsion→dipping →padding or 2 dipping 2 padding
2,Dipping:5-2%(o.w.f) PH=6-7 temperature30-40℃
Time20-30mins drying 80-100℃ curing 130℃
Notice
Adding 0.5-1g/L penetrant or emulsifier to form working solution
Storage and packing
120 kg plastic drum, sealing storage, 6 months at normal temperature
|