Anti-pilling agent
Components:
modified colloidal polysilicic acid
Properties:
Appearance: milky white thick matter
PH value: 6-7
Ionicity: cation
Method:
10-20g/lone-dip one-pad or Two-dip two-pad 100℃pre-drying130℃bakingpadding percent60-80% do experiment before use.