Ningbo Actmix Polymer Ltd. Favorite | Set Home
Curekind Rubber Chemicals
Foamer
Activators
Antioxidants
Curing Agents
Processing aids
Scorch Retarders
Amine Accelerators
Guanide Accelerators
Thiuram Accelerators
Thiourea Accelerators
Thiazoles Accelerators
Sulfenamide Accelerators
Thiocarbamate Accelerators
Actmix Predispersed Masterbatch
Activators
Dessicants
Antioxidants
Accelerators
Curing Agents
Coupling agent
Blowing Agnets
Processing aids
Bonding Systems
Scorch Retarders
Products | Http://www.actmix.cnYour Location:Home » Products

Actmix® Foamer ADC-75

Foamer ADC(AZ)

Active ingredients

 

Azodicarbonamide

Molecular Formula:: C2H4N4O2

Molecular Weight: M.W: 116.08

CAS RN: 123-77-3

EIENCS RN: 204-650-8

Properties:

It can be used for various rubbers, such as CR, EPDM, IIR, NBR(NBR/PVC), and SBR etc. Foamer ADC has high foaming temperature ( 200ˇăC - 210ˇăC).

Use level: 1 - 10 phr.

 

Typical Data:

M.P.: 220-225 oC

Density: 1.65

Purity: 98%

Ash: Max 0.1%

Mean grain size: Max 12um

38µm sieve residue: Max 0.1%

 

High-disperse master batch

Product Name

Active content

%

Color

Filtration

(micron)

Carrier type

Mooney viscosity ML(1+4)

50°C Typical Value

Density

Typical Value

Actmix® ADC-75

75

yellow flake

-

ethylene propylene rubber/EVM

30-50

1.35

* Carrier type can be customized. Except for ethylene propylene rubber/EVM, other carriers, such as nitrile rubber, styrene-butadiene rubber, acrylate rubber and polyepichlorohydrin rubber can be used.

 

Safety & Toxicity:

Pls. refer to related MSDS

Packing & Storage:

25kgs/carton lined with PE bag; 600kgs/pallet

At low temperature (< 35 ˇăC) and dry < 50 % relative humidity), in original packing, closed tight, shelf life is 1 yr.

 

Compared with traditional powdered ADC, Actmix® ADC-75 has the following advantages:

Raw materials 38µm are all under sifting, but no dust appears with master batch

master batch ADC-75 contains small amout of foaming activator, and thus can reduce foaming temperature.

No clay domain appears with master batch at room temperature

Has low Mooney viscosity at low temperature such as 50°C to improve disperse quality

While granulation, master batch can filtering to lower rejection rate.

Has good compatibility with different rubbers
Copyright(C)2009,Ningbo Curekind Polymers Co.,Ltd. All Rights Reserved. Supported by ChemNet ChinaChemNet Toocle Copyright Notice