Ningbo Actmix Polymer Ltd. Favorite | Set Home
Curekind Rubber Chemicals
Thiazoles Accelerators
Sulfenamide Accelerators
Thiuram Accelerators
Guanide Accelerators
Thiourea Accelerators
Amine Accelerators
Curing Agents
Thiocarbamate Accelerators
Antioxidants
Scorch Retarders
Activators
Actmix Predispersed Masterbatch
Accelerators
Blowing Agnets
Antioxidants
Activators
Curing Agents
Dessicants
Bonding Systems
Scorch Retarders
Products | Http://www.actmix.cnYour Location:Home » Products

Curekind® high efficient lubrication auxiliary CUREKIND ST


Introduction:
Ingredients: mixture of high molecular weight unsaturated zinc salts
Appearance: light yellow granules
Density:1.07g / cm3 (20°C)
Ash: 13.0 ± 1 %(850°C2hr)
Melting range:85-100°C
Staining of Vulcanizates : no
Uses: disperse lubrication auxiliary CUREKIND ST the best physical peptizer of natural rubber, is a kind of multifunctional rubber processing auxiliary, can be used in vulcanized rubber to improve anti-reversion properties and heat resistance, with both internal and external lubrication and dispersion function, used in the mastication and mixing process of natural rubber and synthetic rubber; when used in the plastic mastication of rubber, it can peptize natural rubber and isoprene rubber , This product is excellent compatible with rubber, not plastic spray with dual functions of lubrication and peptization. Can improve the processing of rubber, improve the passing rate and dimensional stability of rubber products, reduce energy consumption and improve the efficiency of mixing. In the mixing process of rubber, it can promote the dispersion of fillers and other additives, shorten the mixing cycle, reduce the mixing energy consumption, reduce heat rubber in the use of rubber processing, can improve the extrusion properties of rubber, improve extrusion speed and smoothness of semi-finished.
Application & Dosage:lubricant of highly filled the diolefin kind of synthetic rubber . Especially suitable for containing highly active silica rubber material: tread, industrial molded products .
EPDM, EPM, CPE (CM), HNBR:2 - 3phr
NR, SBR, NBR, IR:1 - 3phr
Safety & Toxicity:Pls. refer to related MSDS
Storage:
sealed tightly, kept in cool, dry and ventilating place, shelf period is 2 years in sealed original packing.
Packing: composite paper bag lined with plastic film bag Net wt 25kg, 500kg/pallet.