Normal technical
condition and depuriating standards
Operational pressure Normal: pressure-3.0MPa
Operational temperature
Airspeed: 500-1000h-1
The percentage of ammonia in the importing raw
materials: 1~10PPm
The percentage of ammonia in the importing raw materials
The ratio between the height of bed and the column diameter:>4
The requirements to meet
the above conditions:
The content of ammonia in the exporting raw materials:
<0.5PPm
The penetration content of ammonia: >5%
Note
1.Condensate water must not be allowed to
flow into the industrial raw materials , so as to prevent
the loss of active constituent.
2.During the operation, sulfur removal must go before
decarbonization.
3.The temperature of the charge gas should be kept at
room temperature. It is bad for reaction to improve
the temperature.
|